Material Notes:
Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt strength, high impact strength, chemical resistance and high stress cracking resistance. It is often used in coextrusion applications.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoUV Stabilizer: YesApplications: Automotive Fuel TanksCompression MoldingsDrumsFood packagingHeavy Gauge SheetIntermediate Bulk ContainersLarge Part Blow MoldingPortable Fuel TanksSmall Engine Fuel TanksThermoformed Parts Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1963
Melt Flow <= 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
5.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Copyright © lookpolymers.com All Rights Reserved