SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.023 cm/cm
0.023 in/in
SABIC Method
0.015 - 0.025 cm/cm

@Time 86400 sec
0.015 - 0.025 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.015 - 0.025 cm/cm

@Time 86400 sec
0.015 - 0.025 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50 mm/min; ISO 527
Elongation at Break 455 %
455 %
50 mm/min; ISO 527
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min; ISO 527
Flexural Yield Strength 12.0 MPa
1740 psi
2 mm/min; ISO 178
Flexural Modulus 0.230 GPa
33.4 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U