Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.3 mmInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
ISO 527-1/-2
Elongation at Break 2.6 %
2.6 %
ISO 527-1/-2
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.770 J/cm²
3.66 ft-lb/in²
ISO 179/1eA
0.650 J/cm²

@Temperature -30.0 °C
3.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
V-0

@Thickness 0.300 mm
V-0

@Thickness 0.0118 in
IEC 60695-11-10
Descriptive Properties Value Comments
Part Marking Code >PBT-GF30FR(17)<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Resin Identification PBT-GF30FR(17)