Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Water Absorption 0.15 %
0.15 %
24 hrs; ASTM D570
Melt Flow 2.3 g/10 min

@Load 1.20 kg,
Temperature 300 °C
2.3 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 122
122
ASTM D785
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Strength 88.3 MPa
12800 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 8.33 J/cm
15.6 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Unannealed (0.125 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed (0.125 in); ASTM D648
Glass Transition Temp, Tg 152 °C
306 °F
Transition Temperature, tested in accordance with ASTM D1525; ASTM E1356
Optical Properties Metric English Comments
Refractive Index 1.585
1.585
ASTM D542
Transmission, Visible 78 %
78 %
125 mil; ASTM D1003
Processing Properties Metric English Comments
Zone 1 229 - 249 °C
445 - 480 °F
Zone 2 241 - 260 °C
465 - 500 °F
Zone 3 249 - 271 °C
480 - 520 °F
Zone 4 249 - 271 °C
480 - 520 °F
Adapter Temperature 246 - 266 °C
475 - 510 °F
Die Temperature 254 - 277 °C
490 - 530 °F
Head Temperature 249 - 271 °C
480 - 520 °F
Zone 2
254 - 277 °C
490 - 530 °F
Zone 1
Mold Temperature 110 - 129 °C
230 - 265 °F
Drying Temperature 121 °C
250 °F
Dry Time 3 - 4 hour
3 - 4 hour
Moisture Content <= 0.020 %
<= 0.020 %
Screw Speed 20 - 40 rpm
20 - 40 rpm
Users viewing this material also viewed the following: