Polymer Property : Screw Speed = 40 rpm Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Speed 15 - 40 rpm
15 - 40 rpm
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..
Screw Speed 20 - 40 rpm
20 - 40 rpm
Entec Hylex® P1302B Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..