Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
PolyOne Maxxam™ PPC-40G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Flexural Strength | 88.3 MPa @Temperature 150 °C |
12800 psi @Temperature 302 °F |
ASTM D790 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Techmer ES Luriblend® TPX-POM-01060 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GA-4025 ABS, 25% Glass Filled Permanent static prevention material with 25% GF reinforcement that can be used in OA device and trayInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GA-4025 ABS, 25% Glass Filled Permanent static prevention material with 25% GF reinforcement that can be used in OA device and trayInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Techmer ES HiFill® PA6 0325 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Daelim H&L Plavis-G40 ISO 40% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 car.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Ensinger Tecapeek® XP-101 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6) Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | ASTM D-790 |
Axiall LR-5009 Rigid PVC, Molding, All Colors Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,.. |
|||
Flexural Strength | 88.3 MPa | 12800 psi | Yeild; ASTM D790 |
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa.. |
|||
Flexural Strength | 88.3 MPa @Thickness 3.17 mm |
12800 psi @Thickness 0.125 in |
ASTM D790 |
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |