Material Notes:
Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
at 24 hours; ASTM D570
Water Absorption at Saturation 6.7 %
6.7 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 49.6 MPa
7200 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Flexural Modulus 1.69 GPa
245 ksi
ASTM D790
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.28
0.28
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 121 µm/m-°C

@Temperature 20.0 °C
67.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 263 °C
505 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Flammability, UL94 HB

@Thickness 0.810 mm
HB

@Thickness 0.0319 in