Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 9.08 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow
Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow
Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FXD103R PC
FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FXD103R PC (Europe-Africa-Middle East)
FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Quantum Polycarbonate
Information provided by Quantum Advanced Engineering Plastics
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
(0.125 in); ASTM D256
M. Holland Company PC406UR Polycarbonate
High impact resistanceGood mold releaseGood UV resistanceHigh viscosityApplications: AppliancesProtective coveringsDecorative displaysHousings
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
0.125 in; 10 mil notch; ASTM D256
Styron CALIBREâ„¢ 301-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
0.125 in; 10 mil notch; ASTM D256
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4310-10 Polycarbonate
EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4330-10 Polycarbonate
EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4510-6 Polycarbonate
EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4530-10 Polycarbonate
EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4530-6 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron CALIBREâ„¢ 2061-6 Polycarbonate
CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and ..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4330-6 Polycarbonate
EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information ..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
Medical grade Zelux GS polycarbonate is produced from resin formulated to meet the stringent performance characteristics and requirements of the healthcare industry. Suitable for EtO gas and limite..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® M Machine Grade Polycarbonate
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® W Window Grade Polycarbonate
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 1021 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 1641 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1641R (with release); 1643 (with UV stabilizers); 1643R (with release and UV stabilizers).Data provided by ..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 527LDMS Nylon 66
A very high impact Nylon 66 with Molybdenum disulfide designed to combine high impact with a reduced co-efficient of friction.Data provided by the manufacturer
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66
A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 1051 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1051R (with release), 1053 (with UV stabilizers), 1053R (with release and UV stabilizers).Data provided by the manufactu..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 1621 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by ..
Copyright © lookpolymers.com All Rights Reserved