Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM55010 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta.. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM55010 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of.. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Technetics Group Amicon™ Acetal Homopolymer