Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 - 80.0 MPa | 7200 - 11600 psi | Average value: 61.7 MPa Grade Count:213 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 49.6 - 75.0 MPa | 7200 - 10900 psi | Average value: 62.8 MPa Grade Count:97 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | ASTM D882 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Techmer ES Statiblend® PBT 03003 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Techmer ES Statiblend® PBT GF10 SS5 MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Techmer ES HiFill® PBT 0150 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Techmer ES Luriblend® POM HO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | ASTM Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ASAPC 122954H Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D-638 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D-638 |
Axiall CL-6380, CL-6380J Rigid PVC, Molding Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | ASTM D-638 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7200 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3500B Description: Blow Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |