Polymer Property : Flexural Strength = 67.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 67.6 MPa
9800 psi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
PolyOne Edgetek® XT XT-500-CX02 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Flexural Strength 67.6 MPa
9800 psi
Perpendicular
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Luriblend® POM CO TL20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composit..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Luriblend® POM CO TS20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS 8004 UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS 8004 UV MB
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS 8012
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS 8014
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Luriblend® POM CO TL20 LE Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS 8004
Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Techmer ES Plastiblend® ABS IM
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Ensinger Tecamid® ST Nylon (PA)
Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc.
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Strength 67.6 MPa
9800 psi
ASTM D-790
Axiall HF-6597 Rigid PVC, Molding
Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide..
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Asahi Kasei Thermylene® P1-10FG-8100 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil