Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.69 GPa | 245 ksi | Tangent; ASTM D790 |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
PolyOne Stat-Tech™ PP-16CP/000-2 HI Polypropylene, Unspecified (PP, Unspecified) Stat-Tech™ electrically conductive compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic applications. These compounds combine .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D 790 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE) Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify i.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | Chord, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1725 Performance Polyolefin Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI71200M High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
BASF Ultramid® 8351 HS BK 102 PA6 (Dry) Description: Ultramid 8351 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM Data |
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
(discontinued **) Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H07B-00 Polypropylene Homopolymer This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 17.. |