Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with very low conductivityhas grades with very low conductivityhas grades with very low compression setgrades with very high abrasion resistanceexcellent tear resistance100% recyclablePVC freeresistance to solventsresistance to oilresistance to acids, bases, and detergentsresistance to UV and ozoneresistance to bacterial and fungus growthhas low toxic potential, with many grades conforming with FDA regulationshalogen free flame retardancycoloured grades availableallows direct colouring during processing by utilizing coloured PP and PE masterbatches2-shot moulding onto many other plasticsappropriate co-extrusion process
Physical Properties Metric English Comments
Density >= 0.890 g/cc
>= 0.0322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Hardness, Shore D 10
10
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Shrinkage 1.0 - 3.5 %
1.0 - 3.5 %
Processing Properties Metric English Comments
Rear Barrel Temperature 170 - 200 °C
338 - 392 °F
Middle Barrel Temperature 170 - 200 °C
338 - 392 °F
Front Barrel Temperature 170 - 200 °C
338 - 392 °F
Die Temperature 180 - 200 °C
356 - 392 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Acid-Base Resistance excellent
Comp. Ratio 2.5 - 3.5
Compression Set good
Draw Down 5-10
Drying not necessary
Injection Speed medium-fast
L/D Ratio 20 - 24:1
Motor Oil Resistance medium
Solvent Resistance medium
UV-Ozone Stability excellent