Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M25UV POM, UV Resistant
(Unverified Data**) Celcon® M25UV is an acetal copolymer developed as a natural UV light stabilized low flow, high molecular weight grade. It has been formulated as a natural acetal that does not discolor, yet maintai.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® UV25Z POM, UV Resistant
(Unverified Data**) Celcon® UV25Z is a nominal 2.5 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® M90LF POM
(Unverified Data**) Hostaform® acetal copolymer grade M90LF is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film.Stan.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 WS 10/1570 POM, UV Resistant
(Unverified Data**) Preliminary Data SheetImpact modified, weatherableInformation provided by Celanese |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | Extrusion |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Die Temperature | 160 - 200 °C | 320 - 392 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® GC15 POM, 15% Glass Reinforced Celcon« GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.Information provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® XT 20 POM, Impact Modified Preliminary Data SheetInformation provided by Celanese |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® C 9021 XAP² POM, Unfilled POM copolymerrecommendedInformation provided by Celanese Corporation. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® CF802 POM, Specialty Celcon« acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon« CF802 has been developed to dissipate static electricity from fuel handling systems... |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M25UV POM, UV Resistant Celcon« M25UV is an acetal copolymer developed as a natural UV light stabilized low flow, high molecular weight grade. It has been formulated as a natural acetal that does not discolor, yet maintai.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M450 POM, Unfilled Celcon« acetal copolymer grade M450 is an extremely low viscosity grade for optimal cycle performance in very thin walls or long, narrow flow paths in injection molding.Information provided by Cela.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Celcon® MR25B POM, Specialty Celcon« MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified Hostaform« acetal copolymer grade S 9363 XAP2 Ö is an impact modified grade for demanding applications. Hostaform« S 9363 XAP2 Ö provides good impact strength while improving modulus and weld.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9363 XAP2 ™ POM, Impact Modified Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® MC90 POM, Mineral Reinforced
(Unverified Data**) Celcon® acetal copolymer grade MC90 is a mineral reinforced grade offering low warp, improved dimensional stability, improved stiffness, improved practical impact and retention of other base resin .. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 27064 POM, Impact Modified
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POM-HIEasy flowing, elastomer-containing injection molding grade, high toughnessInformation provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
(Unverified Data**) Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® XT 90 POM, Impact Modified
(Unverified Data**) Preliminary Data SheetHighly impact modified, improved weld lineInformation provided by Celanese |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® LW90-F2 POM, Tribological Celcon« LW90-F2 is an acetal copolymer formulated with a nominal 9 melt flow rate base polymer and a standard level of polytetrafluoroethylene filler (PTFE). It is designed for use in wear applicat.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant PolyacetalcopolymerInformation provided by Celanese |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® CF802 10/9022 POM, Specialty Hostaform« acetal copolymer grade CF802 10/9022 is a conductive, fuel compatible general purpose acetal copolymer. Hostaform« CF802 10/9022 has been developed to dissipate static electricity from .. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M90AW POM, Tribological Celcon« M90AW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear in low load-high velocity applications. Celcon« M90AW is an option .. |