Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 170 °C | 338 °F | |
Multibase TPSiV™ 3040-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 170 - 185 °C | 338 - 365 °F | Injection Molding |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |
|||
Rear Barrel Temperature | 170 - 185 °C | 338 - 365 °F | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 170 - 180 °C | 338 - 356 °F | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 170 - 220 °C | 338 - 428 °F | Injection or Extrusion |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Aft-1. Region Temperature |
Tisan TISETILEN® Flame Retardant (V0) Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Rear Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Rear Barrel Temperature | 170 - 220 °C | 338 - 428 °F | Injection or Extrusion |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |