Material Notes:
Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 2865PE can be overmolded and coextruded with polyethylene.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.014 - 0.024 cm/cm
0.014 - 0.024 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ASTM D2240
Tensile Strength 7.70 MPa
1120 psi
ASTM D412
Elongation at Break 588 %
588 %
ASTM D412
100% Modulus 0.00243 GPa
0.352 ksi
ASTM D412
Compression Set 17 %

@Temperature 20.0 °C,
Time 79200 sec
17 %

@Temperature 68.0 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature <= 79.4 °C
<= 175 °F
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Front Barrel Temperature 182 - 188 °C
360 - 370 °F
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi
Descriptive Properties Value Comments