Mechanical Properties Metric English Comments
Tensile Strength 7.72 MPa

@Strain 100 %
1120 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3816 Polyvinyl Chloride, Flexible (PVC, Flexible)
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of..
Tensile Strength 7.70 MPa
1120 psi
Momentive Performance Materials FSE7520 Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 7.72 MPa
1120 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1126 P (SIS) Radial Copolymer
Description: Kraton D1126 P is a clear, radial copolymer based on styrene and isoprene, with a polystyrene content of 21%. In addition, it has a diblock content of 30% and high melt flow. It is supp..
Tensile Strength 7.70 MPa
1120 psi
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer
KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Tensile Strength 7.70 MPa
1120 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer
Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for..
Tensile Strength 7.70 MPa
1120 psi
300; ISO 37
BASF Elastoblend LP 9192 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 7.70 MPa
1120 psi
ISO 37
AlphaGary Evoprene™ Super G 949 SEBS Thermoplastic Elastomer