Processing Properties Metric English Comments
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Oxford Polymers C-Acetal 10MF-900 BK Acetal
Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford..
Nozzle Temperature 182 - 204 °C
360 - 400 °F
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 204 °C
360 - 400 °F
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer
Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer
Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer
Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer
Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer
Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer
Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer
Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer
Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8048N Thermoplastic Elastomer
Elastocon® 8048N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8048N is FDA compliant and well suited..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer
Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer
Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer
Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer
Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer
Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer
Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer
Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer
Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited..
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer
Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer..
Nozzle Temperature 185 - 204 °C
365 - 400 °F
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer
Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer
Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer
Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer
Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer
Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer
Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela..