Lendell Manufacturing Prepol Pre Polymer

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Lendell Manufacturing Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lendell Manufacturing Prepol Pre Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Liquid Apperance, Amber, honey likePolyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 80% by weight and a very low exotherm reaction.Applications:Cosmetic, Consumer Products, Filtering, Medical, Agricultural, Wicking, Thermal, Acoustical, Wiping, Industrial, Insulations, Fire Protection, Sports/Leisure, Cushioning, Flotation, Automotive, Anti-Static, ToysFoam Additives:Colors, Fragrances, All Liquids, Solids, Abrasives, Microbicides - Live AlgaeInformation provided by Lendell Manufacturing Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Viscosity 3000 cP

@Temperature 45.0 °C
3000 cP

@Temperature 113 °F
8000 cP

@Temperature 31.0 °C
8000 cP

@Temperature 87.8 °F
12500 cP

@Temperature 25.0 °C
12500 cP

@Temperature 77.0 °F
34000 cP

@Temperature 17.0 °C
34000 cP

@Temperature 62.6 °F
Thermal Properties Metric English Comments
Melting Point 14.4 °C
58.0 °F
Flash Point 232 °C
450 °F
Descriptive Properties Value Comments
% Free Toluene Diisocyanate >4
% NCO content 8.5
Equivalent Wt (per NCO) 475
NCO (meq/g) 2.11