Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1020 GP is a 20% talc reinforced polypropylene homopolymer. It has applications in general purpose industrial, automotive, consumer, and construction.Data provided by Composite Technologies.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Back Pressure | 0.689 MPa | 100 psi | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® OF65 Thermoplastic Elastomer Elastocon® OF65 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a reduced coefficient of f.. |