Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar EN001 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar EN001 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming. Eastar EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.Applications/UsesFood PackagingHousewaresToys/Sporting goodsWriting instruments
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
114
114
ISO 2039-2
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 527
25.0 MPa
3630 psi
ASTM D638
Tensile Strength, Yield 57.0 MPa
8270 psi
ISO 527
58.0 MPa
8410 psi
ASTM D638
Elongation at Break 120 %
120 %
ISO 527
120 %
120 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ISO 527
2.40 GPa
348 ksi
ASTM D638
Flexural Yield Strength 77.0 MPa
11200 psi
ISO 178
84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 3.10 kJ/m²

@Temperature -40.0 °C
1.48 ft-lb/in²

@Temperature -40.0 °F
ISO 180
4.50 kJ/m²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO) NB
NB
ISO 180
170 kJ/m²

@Temperature -40.0 °C
80.9 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Puncture Energy 0.800 J

@Thickness 2.50 mm,
Temperature -40.0 °C
0.590 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ISO 6603-2
1.00 J

@Thickness 3.20 mm,
Temperature -40.0 °C
0.738 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ISO 6603-2
1.60 J

@Thickness 2.50 mm,
Temperature -40.0 °C
1.18 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
2.10 J

@Thickness 3.20 mm,
Temperature -40.0 °C
1.55 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ASTM D3763
15.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
11.1 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ISO 6603-2
18.0 J

@Thickness 3.20 mm,
Temperature 23.0 °C
13.3 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
max load; ISO 6603-2
26.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
19.2 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ASTM D3763
31.0 J

@Thickness 3.20 mm,
Temperature 23.0 °C
22.9 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ISO 75
69.0 °C
156 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75
65.0 °C
149 °F
ASTM D648
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 84 %
84 %
Total Transmittance; ASTM D1003
Copyright © lookpolymers.com All Rights Reserved