Mechanical Properties Metric English Comments
Izod Impact, Notched 0.270 J/cm

@Thickness 3.18 mm,
Temperature 0.000 °C
0.506 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Izod Impact, Notched 0.270 J/cm

@Temperature -30.0 °C
0.506 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar GN125 Copolyester, Natural  (discontinued **)
Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co..
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
50%RH; ASTM D256
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar EN001 Copolyester
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro..
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar MN021 Copolyester
Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Izod Impact, Notched 0.270 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.506 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade
Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr..
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..