Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.54 g/cc
0.309 lb/in³
Thermal Properties Metric English Comments
Melting Point 79.0 °C
174 °F
Eutectic
Solidus 79.0 °C
174 °F
Liquidus 79.0 °C
174 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 57 %
57 %
Indium, In 26 %
26 %
Tin, Sn 17 %
17 %