Polymer Property : Puncture Energy = 2.10 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.10 J

@Thickness 3.20 mm,
Temperature -40.0 °C
1.55 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Puncture Energy 2.10 J

@Temperature -30.0 °C
1.55 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Puncture Energy 2.10 J

@Thickness 3.20 mm,
Temperature -40.0 °C
1.55 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman Eastar EN001 Copolyester
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro..
Puncture Energy 2.10 J

@Thickness 3.20 mm,
Temperature -40.0 °C
1.55 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman Eastar MN021 Copolyester
Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Puncture Energy 2.10 J

@Thickness 3.20 mm,
Temperature -40.0 °C
1.55 ft-lb

@Thickness 0.126 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..