Eastman E6838-850P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman E6838-850P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seals at high packaging or sealing rates. It also demonstrates a good adhesion to paper, provides a good moisture barrier and is heat-sealable at low temperatures.List of Applications:Coatings for paper/paperboardFood-contact applicationsInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ASTM D4883
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.70 MPa
1410 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 400 %
400 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating