Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.172 GPa | 24.9 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 811A Polyethylene
(discontinued **) Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 811E Polyethylene
(discontinued **) Extrusion grade; no additives. 811E as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1).Information from manufacturer data sheet.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 811P Polyethylene
(discontinued **) Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman M3018-P Polyethylene
(discontinued **) Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various .. |
|||
Flexural Modulus | 0.172 GPa | 25.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | ASTM D790 |
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | ASTM D412 |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
Flexural Modulus | 0.172 GPa | 25.0 ksi | ASTM D790 |
Ecomass® 4703BI74 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | ASTM D790 |
Asia Technology Pioneers CAP 101 PP Nanocomposite Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Modulus | 0.172 GPa | 24.9 ksi | ASTM D790 |
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in.. |