Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.72 MPa | 1410 psi | ASTM D412 |
Polymax® Maxelast® D6780 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 9.72 MPa | 1410 psi | ASTM D412 |
Polymax® Maxelast® F7880 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Strength, Yield | 9.70 MPa | 1410 psi | 500 mm/min; ASTM D638 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Tensile Strength, Yield | 9.70 MPa | 1410 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 808E Polyethylene
(discontinued **) Low density polyethylene 808E is a general-purpose formulation used general-purpose extrusion. Under regulations administered by the US FDA, 808E may lawfully be used as articles or components of a.. |
|||
Tensile Strength, Yield | 9.70 MPa | 1410 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Tensile Strength, Yield | 9.70 MPa | 1410 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman E6838-862A Polyethylene
(discontinued **) E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic.. |
|||
Tensile Strength, Yield | 9.72 MPa | 1410 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 600 Perfluoroelastomer Chemraz® 600, a perfluoroelastomer, works well in both high and low temperatures. It is capable of withstanding temperatures raging from -4°F to 500°F (-20°C to 260°C). Additionally.. |
|||
Tensile Strength, Yield | 9.72 MPa | 1410 psi | ASTM D412 |
Teknor Apex Flexalloy® 3500-50 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 9.70 MPa | 1410 psi | Molded property |
Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging ap.. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 50.0 % |
1410 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |