Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 24.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.172 GPa
24.9 ksi
ASTM D790
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman E6838-889P Polyethylene  (discontinued **)
Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat..
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 811A Polyethylene  (discontinued **)
Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol..
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 811E Polyethylene  (discontinued **)
Extrusion grade; no additives. 811E as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1).Information from manufacturer data sheet..
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 811P Polyethylene  (discontinued **)
Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol..
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman E6838-850P Polyethylene  (discontinued **)
E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal..
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman M3018-P Polyethylene  (discontinued **)
Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various ..
Flexural Modulus 0.172 GPa
24.9 ksi
ASTM D790
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Flexural Modulus 0.172 GPa
24.9 ksi
ASTM D412
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in ..
Flexural Modulus 0.172 GPa
24.9 ksi
ASTM D790
Asia Technology Pioneers CAP 101 PP Nanocomposite
Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..
Flexural Modulus 0.172 GPa
24.9 ksi
ASTM D790
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..
Copyright © lookpolymers.com All Rights Reserved