Material Notes:
Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resistanceGood adhesion to Polymer Optical Fibers (POF)Low influence on the dampening of the transmission of optical fibersLow density, low weight Grilamid XE 3926 black 9992 is especially suitable for high speed extrusion of thin walled inner sheathings for polymer optical fibers (POF).Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 MPa
10200 psi
conditioned; ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa
160 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Processing Injection Molding
Other Extrusion
Product Attributes Improved flowability and demoulding