Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D resin is designed to run on narrow die-gap equipment. It contains medium levels of slip additive and antiblock additive. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.1 (a) for food packaging applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Thickness 38.0 microns
1.50 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
Film Tensile Strength at Yield, TD 12.0 MPa
1740 psi
Coefficient of Friction 0.17
0.17
Elmendorf Tear Strength MD 560 g
560 g
Elmendorf Tear Strength TD 1050 g
1050 g
Elmendorf Tear Strength, MD 14.7 g/micron
373 g/mil
Elmendorf Tear Strength, TD 27.6 g/micron
701 g/mil
Dart Drop 6.60 g/micron
168 g/mil
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
Film Tensile Strength at Break, TD 35.0 MPa
5080 psi
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C
221 °F
Optical Properties Metric English Comments
Haze 10 %
10 %
Gloss 39 %
39 %
45°
Processing Properties Metric English Comments
Processing Temperature 226 °C
439 °F
Film extrusion temperature
Copyright © lookpolymers.com All Rights Reserved