Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA reg.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of .. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high .. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2071 Linear Low Density Polyethylene DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Processing Temperature | 226 °C | 439 °F | Film extrusion temperature |
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2267A Polyethylene resin is a high performance blown film polymer offering superior load retention and toughness for a variety of stretch film packaging applications. This material complies.. |