Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength TD = 1050 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 1050 g

@Thickness 0.0254 mm
1050 g

@Thickness 0.00100 in
ASTM D1922
Total 9458 HDPE Film Grade
Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba..
Elmendorf Tear Strength TD 1050 g
1050 g
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r..