| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning 748 NON-CORROSIVE SEALANT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc <br>@Temperature 25.0 °C |
1.33 g/cc <br>@Temperature 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 35 | 35 | |
| Tensile Strength, Ultimate | 1.90 MPa | 275 psi | |
| Elongation at Break | 350 % | 350 % | |
| Peel Strength | 4.38 kN/m | 25.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 177 °C | 351 °F | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.70e+14 ohm-cm | 7.70e+14 ohm-cm | |
| Dielectric Constant | 3.21 <br>@Frequency 100000 Hz |
3.21 <br>@Frequency 100000 Hz |
|
| 3.3 <br>@Frequency 100 Hz |
3.3 <br>@Frequency 100 Hz |
||
| Dissipation Factor | 0.0028 <br>@Frequency 100000 Hz |
0.0028 <br>@Frequency 100000 Hz |
|
| 0.0087 <br>@Frequency 100 Hz |
0.0087 <br>@Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 2160 min <br>@Temperature 22.0 °C |
36.0 hour <br>@Temperature 71.6 °F |
|
| Shelf Life | 24.0 Month | 24.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | off-white | |
| Flowable | no | |
| Water Resistant | yes |