Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 4.38 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 4.38 kN/m
25.0 pli
PP; overmold failure; 90 degrees, 20 in/min (500 mm/min); ISO 813
RTP Company RTP 2700 S-30A Saturated Styrenic Block Copolymer, General Purpose
Peel Strength 4.38 kN/m
25.0 pli
T-peel
Master Bond EP21TDCANHT Two Component Thermally Conductive, Electrically Insulative Epoxy Adhesive
Product Description: EP21TDCANHT is a two component, flexibilized, thermally conductive epoxy adhesive that will cure at room temperature, or more rapidly at elevated temperature. It is a good adhes..
Peel Strength 4.38 kN/m
25.0 pli
T-peel, Al to Al
Master Bond Supreme 11LP Epoxy Resists Impact and Thermal Shock
Description: This two component adhesive system is formulated to cure at room temperature or more rapidly at elevated temperatures, with a mix ratio (part A/part B: 100/100). Master Bond Polymer Adh..
Peel Strength 4.38 kN/m
25.0 pli
Dow Corning 748 NON-CORROSIVE SEALANT
White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning
Peel Strength 4.38 kN/m
25.0 pli
Bond Strength (S1 to S1); Arlon SQA-TMS-011
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a..
Peel Strength 4.38 kN/m
25.0 pli
Bond Strength; ASTM D624
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5816 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ5832 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5904 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
3M Bumpon™ SJ5904 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M Bumpon™ SJ6008 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
3M Bumpon™ SJ6008 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M Bumpon™ SJ6016 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ6032 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
3M SJ5400 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M SJ5500 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M SJ5500 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M SJ5700 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
3M Bumpon™ SJ5916 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
T-Peel, Aged 71°C for 2 weeks, Substrate failure
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M Bumpon™ SJ5808 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Peel Strength 4.38 kN/m
25.0 pli
Al to Al
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..
Peel Strength 4.38 - 5.26 kN/m
25.0 - 30.0 pli
T-peel, Al to Al
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures
Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen..
Peel Strength 4.38 kN/m
25.0 pli
PP; Failure at interface; 90 degrees, 20 in/min (500 mm/min); ISO 813
RTP Company RTP 2700 S-80A Saturated Styrenic Block Copolymer, General Purpose
Copyright © lookpolymers.com All Rights Reserved