Techmer ES Luriblend® PA6 TSX15 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, PTFE Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PA6 TSX15 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 69.6 MPa
10100 psi
ASTM D638
Elongation at Yield 25 %
25 %
ASTM D638
Flexural Yield Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 171 °C
340 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Unannealed; ASTM D648