Mechanical Properties Metric English Comments
Peel Strength 4.38 kN/m
25.0 pli
Polypropylene; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
RTP Company RTP 2700 S-80A Z Saturated Styrenic Block Copolymer (TES/SEBS or other), FDA Compliant Ingredients
Peel Strength 4.38 kN/m
25.0 pli
Dow Corning 748 NON-CORROSIVE SEALANT
White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning
Peel Strength 4.38 kN/m
25.0 pli
Bond Strength (S1 to S1); Arlon SQA-TMS-011
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a..
Peel Strength 4.38 kN/m
25.0 pli
Bond Strength; ASTM D624
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ5816 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M Bumpon™ SJ5816 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5816 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ5832 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M Bumpon™ SJ5904 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5908 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M Bumpon™ SJ5908 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ6016 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
3M Bumpon™ SJ6016 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M SJ5300 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M SJ5400 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M SJ5500 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M SJ5500 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polystyrene
3M SJ5700 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M SJ5700 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5916 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
3M Bumpon™ SJ5916 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
T-Peel, Aged 71°C for 2 weeks, Substrate failure
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to Polypropylene
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 4.38 kN/m
25.0 pli
90°, Adhesion to ABS
3M Bumpon™ SJ5808 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Peel Strength 4.38 kN/m
25.0 pli
T-Peel
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Peel Strength 4.38 kN/m
25.0 pli
PP; Failure at interface; 90 degrees, 20 in/min (500 mm/min); ISO 813