Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol PL 795SF Composite Surfacing Film Modified epoxy film specifically formulated to improve the surface appearance of composite honeycomb structures. Excellent surface appearance; reduced pinholing, extra finishing. Superior out-time. .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Dow Corning 748 NON-CORROSIVE SEALANT White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco Delo® NLGI 1 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco Delo® NLGI 2 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | See Note 2. |
ChevronTexaco EP 1 Aluminum Complex Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for addition.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco NLGI 2 Moly MAX Grease EP FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | See Note 2. |
ChevronTexaco Starplex® Moly NLGI Grade 1 Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco Rykon® 1426 Premium Grease Chevron Rykon Premium Grease No. 1426 contains polyurea thickener, highly refined paraffinic base oil, rust and oxidation inhibiting additives, as well as heatstable extreme pressure additives.Appli.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | See Note 2. |
ChevronTexaco Starplex® NLGI Grade 1 Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
3M 1675 Polyester Protective Tape 3M™ Polyester Protection Tape 1675 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Long term |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9593 Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | Short term |
3M 9731 Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol EA 9845 SF Composite Surfacing Film Epoxy-based composite surfacing film improves surface quality of honeycomb stiffened composite parts. Reduced weight vs conventional surfacing films. Cures at 250°F/121°C or 350°F/177°C with a v.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol PL 795 Film Adhesive Epoxy film adhesive designed for composite bonding applications. May cure at 250°F / 121°C or 350°F / 177°C, with service temperatures up to 350°F / 177°C. Ideal for co-cure or secondary bondi.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco Rykotac® Grease EP FeaturesChevron Rykotac Grease EP is manufactured using highly refined, select high viscosity index base oils, and a polyurea thickener. It is red in color and tacky in texture.Chevron Rykotac Greas.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Maximum Service Temperature, Air | >= 177 °C | >= 351 °F | |
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol EA 9394 Paste Adhesive System Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol EA 9820 Paste Adhesive System High-density, one-component epoxy syntactic for use on honeycomb composite parts requiring high compressive strength at temperatures up to 350°F / 177°C. Ideal for fastener or attachment potting a.. |
|||
Maximum Service Temperature, Air | 177 °C | 351 °F | |
Henkel Hysol PL 460 Core Splice Adhesive Foaming epoxy adhesive in paste form for easy extrusion through packaged cartridges. Expands and cures at temperatures from 250°F / 121°C to 350°F / 177°C. Qualified to Boeing BMS 5-90, Type IV... |