Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.70e+14 ohm-cm | 7.70e+14 ohm-cm | |
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting.. |
|||
Volume Resistivity | 7.70e+14 ohm-cm | 7.70e+14 ohm-cm | |
Dow Corning 748 NON-CORROSIVE SEALANT White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning |