Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
chs 0.2 in/min; ASTM D638
Elongation at Yield 3.0 %
3.0 %
chs 0.2 in/min; ASTM D638
Flexural Modulus 5.27 GPa
764 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
0.125";; ASTM D648
Descriptive Properties Value Comments
Glass Content (%) 30
ASTM D2584