Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | Unannealed; ISO 75-2/A |
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO 75-1/-2 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 - 180 °C | 311 - 356 °F | ISO 75-A |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 - 180 °C | 311 - 356 °F | Injection and Compression; ISO 75-A |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO 75-1/-2 |
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | |
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PBT/ABS GF/M40 FR 40/40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Fiber Reinforcement, 40/40% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C @Thickness 3.20 mm |
311 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C @Thickness 3.20 mm |
311 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 - 175 °C | 311 - 347 °F | ISO 75 Af |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | Absolute Drying; ASTM-D648 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Toyobo T-772 Nylon, Plating Grade Key Feature: Plating grade; Glass fiber and mineral reinforced grades; thermal and impact resistantInformation provided by Toyobo Co., Ltd |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | 0.125";; ASTM D648 |
Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO 75 |
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ASTM D648 |
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO 75/2a |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO 75-1/-2 |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | |
LATI Latilub 88/50-20T PEEK, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 155 °C | 311 °F | ISO75A |
Panjin Zhongrun Chemerize 021G Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |