Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.27 GPa | 765 ksi | Tangent; ASTM D790 |
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.27 GPa | 765 ksi | Tangent; ASTM D790 |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.27 GPa | 765 ksi | Tangent; ASTM D790 |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | ISO 178 |
Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL Â.. |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | ISO 178 |
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | ASTM D790 |
Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 5.27 GPa | 764 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific) PPE/PS, GF20%, high heat, non-FR |