Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2000 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2000 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under component file E40654. 02000 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.32 %
0.32 %
ASTM D570
Linear Mold Shrinkage 0.0065 cm/cm
0.0065 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 0.67 %
0.67 %
ASTM D638
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Flexural Strength 81.0 MPa
11700 psi
ASTM D790
Flexural Modulus 7.10 GPa
1030 ksi
ASTM D790
Compressive Strength 214 MPa
31000 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 2.89 GPa
419 ksi
Calculated
Izod Impact, Notched 0.181 J/cm
0.339 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.195 J/cm²
0.928 ft-lb/in²
ASTM D256
Impact 98
98
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 197 °C
387 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 27 %
27 %
ASTM D2863
Shrinkage 0.21 %
0.21 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+11 ohm-cm
2.70e+11 ohm-cm
ASTM D247
Dielectric Constant 6.1
6.1
ASTM D150
Dielectric Strength 8.60 kV/mm
218 kV/in
Short Time; ASTM D149
Dissipation Factor 0.065
0.065
ASTM D150
Arc Resistance 117 sec
117 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638