Mechanical Properties Metric English Comments
Flexural Modulus 5.27 GPa
764 ksi
ISO 178
Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL Â..
Flexural Modulus 5.27 GPa
764 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific)
Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only
Flexural Modulus 5.27 GPa
764 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp ZWM2411 PPE+PS (Asia Pacific)
Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color onlyThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 5.27 GPa
764 ksi
ISO 178
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 5.27 GPa
764 ksi
ASTM D790
Diamond Polymers NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 5.27 GPa
764 ksi
ASTM D790
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific)
PPE/PS, GF20%, high heat, non-FR