Diamond Polymers ASA/PC 7030

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA/PC 7030.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 56.80 MPa
8238 psi
chs 2 in/min; ASTM D638
Flexural Modulus 2.47 GPa
358 ksi
Procedure B, Test Method I(chs 0.05 in/min); ASTM D790
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 109 °C
228 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 139 °C
282 °F
0.125 inch, 1 Kg; ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in