Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 358 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® MG37EPX ABS
ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L)
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® MG37EPX ABS (Europe-Africa-Middle East)
ABS plating grade optimized for a broad processing window for both painted and plated applications.
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free..
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 2.47 GPa
358 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Flexural Modulus 2.47 GPa
358 ksi
ASTM D 790
MRC Polymers NAXALOYâ„¢ 774 ABS + PC Alloy
• Alternative to high heat ABS resins• For injection molding• Excellent heat and impact resistanceInformation provided by MRC Polymers Inc.
Flexural Modulus 2.47 GPa
358 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6
LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.47 GPa
358 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific)
LNP* Lubricomp* ZP001XXP is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.47 GPa
358 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH7010 PPE+PS
Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts..
Flexural Modulus 2.47 GPa
358 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific)
High heat, Non halogenated flame retardant Noryl product
Flexural Modulus 2.47 GPa
358 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Flexural Modulus 2.47 GPa
358 ksi
Procedure B, Test Method I(chs 0.05 in/min); ASTM D790
Diamond Polymers ASA/PC 7030
Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved