Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ASTM D648 |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C @Thickness 3.20 mm |
228 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp NL002 PC+ABS (Europe-Africa-Middle East) LNP* Lubricomp* PCAL4020S is a compound based on PC+ABS Blend resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C @Thickness 3.20 mm |
228 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C @Thickness 3.20 mm |
228 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C @Thickness 6.40 mm |
228 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75 |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75 |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL N1150 PPE+PS Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C @Thickness 6.40 mm |
228 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PX1340 PPE+HIPS (Asia Pacific) PPE+PS MF Filled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® S3100 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75-1,-2 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75-1/-2 |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75-1/-2 |
Covestro Bayblend® T85 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ISO 75-1/-2 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | |
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS TX-541 Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA/PC 7030 Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ASTM D648 |
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Method A - Annealed; ASTM D-648 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Method A - Annealed; ASTM D-648 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 109 °C | 228 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |