Polymer Property : Tensile Strength, Yield = 56.80 MPa
Polymer Property :
Tensile Strength, Yield =
56.80 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
56.80
MPa
8238
psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA/PC 7030
Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc.