Polymer Property : Izod Impact, Notched = 4.70 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
Nylene® Norpex® AX300 PPE (Polyphenylene Ether); Premium Performance High Heat
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS
High flow PC+ABS material designed for local Pacific Automotive applications
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific)
High flow PC+ABS material designed for local Pacific Automotive applications
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® BFL4000U PC
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
ASTM D256
I. Stern 745 Super High Impact Natural ABS
Features:Super High ImpactExtrusionApplicationsPipeProfilesSheetInformation provided by I. Stern & Co. Inc.
Izod Impact, Notched 4.70 J/cm

@Thickness 3.17 mm
8.81 ft-lb/in

@Thickness 0.125 in
ASTM D256
Hannam Chemical Hanalac 795 ABS, Pipe Grade
Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity.
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
Partial break; ASTM D256
Ineos K44-11-128 HDPE
Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi..
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Diamond Polymers ASA/PC 7030
Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
ASTM D256
Aclo Accucomp ABS ABS804L High Impact Grade
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
Custom Resins Norpex® 300 PPE (Polyphenylene Ether)  (discontinued **)
Premium performance high heat. Properties for dry as molded samples.Data provided by the manufacturer