Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS (Europe-Africa-Middle East) ABS plating grade optimized for a broad processing window for both painted and plated applications. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free.. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | ASTM D 790 |
MRC Polymers NAXALOY™ 774 ABS + PC Alloy • Alternative to high heat ABS resins• For injection molding• Excellent heat and impact resistanceInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific) LNP* Lubricomp* ZP001XXP is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Flexural Modulus | 2.47 GPa | 358 ksi | Procedure B, Test Method I(chs 0.05 in/min); ASTM D790 |
Diamond Polymers ASA/PC 7030 Description: ASA/Polycarbonate AlloyInformation provided by Diamond Polymers, Inc. |