DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Flame Retarded + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
(DAM); ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179/1eU
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
(DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Comparative Tracking Index 325 V
325 V
IEC 60112